Metal Crack Stitching
©2012 Metal Crack Stitching ©2012 Metal Crack Stitching   ©2012 Metal Crack Stitching Back to Home ©2012 Metal Crack Stitching   Before and After Photos ©2012 Metal Crack Stitching Contact Us ©2012 Metal Crack Stitching ©2012 Metal Crack Stitching
©2012 Metal Crack Stitching
�2012 Metal Crack Stitching

Before/After Photos

Click on any image for a close-up look (pop-up window)
Before After
Cast Aluminum (Split in half)
Metal stitched and restored lost strength
Before After
700 Ton Injection Molder (Cast steel)
1�" - thick cast steel cracked.
Repaired with the superkey and stitch combination.
Before After
Shear Frame (Cast Iron)
With a capacity to shear �" thick x 12' long steel plate. Frame cracked separated. Repaired utilizing superkeys and stitch combination.
Before After
Trunion Roll (Cast Steel)
9" thick spoke cracked.
Repaired using metal stitching system.
Before After
Gear Box
Before During
400 Ton Press Break Crack Previously Welded
Before After
50 Ton Punch Press
Before
Kiln Tire From a Major Cement Plant Hydro Turbine
Ajax 2500 Ton Forging Press
AJAX 2500 TON FORGING PRESS COLUMN CRACKED AJAX 2500 TON FORGING PRESS BASE
Sketch of a large Circulating Water Pump, weighs approximately 30 ton, with 65 feet of crack. Metal stitched and sealed.
Circulating Water Pump
Before After
Wire/Cable Stripper Gear Housing
Coal Feeder From a Power Plant Ship Generator Engine Block Compressor